Maintaining stable power output in cold environments is an important potential application of sodium-ion batteries. In Grepow's internal R&D testing, a sodium-ion cell was fully charged, held at -30°C for four hours, and then subjected to repeated 20C pulse discharges lasting three seconds each.
In a separate test, the cell completed repeated 28C pulse discharges lasting three seconds each after a four-hour soak at -20°C. These results provide preliminary engineering references for applications requiring short-duration power in cold environments.

Grepow also tested a sodium-ion development cell at 25°C using a 1C charge rate and a 30C discharge rate. After 2,000 cycles under these conditions, the cell retained 94% of its original capacity.
Based on the interim test curve currently available, if capacity fade does not accelerate significantly, the cell could exceed 4,000 cycles before capacity retention falls to 80%.

Sodium-Ion Pouch Cells: Low-Temperature, High-Pulse and Long Cycle Life